2010年7月9日 星期五

自製SDS PAGE 板


昨天本來要做個 Western Blot, 於是開始找玻璃板來做gel.
結果好死不死本實驗室做 SDS gel 的板子很多都破了不能用,
由於這套系統的原產地是日本,所以要買新的板子還要跟日本訂,運過來還要付運費......
加上買新的還是有可能打破,那就自己用塑膠板切一個吧XD.
Yesterday I wanted to do a Western blot, so I was looking for glass plates.
However, in our lab several SDS PAGE glass plates were broken.
Because this SDS PAGE system came from Japan, we need place order from Japan and plus shipping......
Besides, new glass plate still could be destroyed, so I decided make one for myself from plastic plate. XD.


於是直接拿舊的做模子,關鍵的點標一標,線畫一畫然後開始用鋸子切.
So, I used old glass plate as template, mark essential point and draw lines, then cut the plate by saw.

切完收工,左邊是舊的,右邊是我切的......看起來OK吧.
Finish, the one on left is old glass plate, the one on the right is I made......
Looks OK.


試跑看看......(剛好在純化蛋白,就拿來試一試)
Test run my recent purified protein.

跑完之後染色看起來OK嘍.
After electrophoresis stain the gel, Looks OK.

注意事項:由於塑膠製品比較軟,所以安裝gel時要小心,可能會有氣泡,如果直接在架子上做gel應該可以排除這個問題.
By the way, because the plastic is much softer than glass, bubble might form when you assemble the gel to the apparatus. It should not be problem if you fix the plates on apparatus then make the gel.

2010年5月7日 星期五

Absorbed Glass Mat Battery(AGM電池) On Venox

最近幾次發車(Venox)馬達越轉越沒力,最後就是繼電器的聲音,我有試著把電瓶拿下來用1A充電,充到12.8V後裝回是可以發動,裝回車上發動後電壓都有13~14V(應該不是發電機的問題吧)。只是大概騎兩天電瓶又沒電了,想想這顆電瓶也用了六年大概也不行了,想說買一顆來換。美國這最近流行一種(Absorbed Glass Mat)AGM電瓶,號稱壽命是一般電瓶的2~3倍,硫酸吸附在Glass Mat中,就算把電池切開也不會漏。有能力把充電時產生的氫氣,氧氣直接在電瓶內結合還原成水,真正免加水。後來我跑去WALMART買了GS的AGM電瓶(台灣製)。看了一下廠商的介紹,除了硫酸吸附在Glass Mat之外還有一些強化措施:電極改用鉛鈣合金加上結構上也有補強更耐震,新配方的硫酸不會在電極上型成硫化物能降低內阻。我買的電瓶要自己灌硫酸,灌完擺一小時,再用1A充兩小時就可以用了。新電瓶裝上車馬達力道又回復正常,電力有沒有比較強短期內還看不出來,看看能不能用個十年......
最後提醒一下美國這買電瓶要付押金9美金,買新電瓶記得帶舊的去,可以抵掉押金。